This alloy typically has a tin content ranging from 0.5% to 1.0%, and a phosphorous range of 0.01% to 0.35%. These alloys are notable for their toughness, strength, low coefficient of friction, high fatigue resistance, and fine grain. The tin content increases the corrosion resistance and tensile strength, while the phosphorous content increases the wear resistance and stiffness. Some typical end uses for this product would be electrical products, bellows, springs, washers, corrosion resistant equipment
This alloy typically has a tin content ranging from 0.5% to 1.0%, and a phosphorous range of 0.01% to 0.35%. These alloys are notable for their toughness, strength, low coefficient of friction, high fatigue resistance, and fine grain. The tin content increases the corrosion resistance and tensile strength, while the phosphorous content increases the wear resistance and stiffness. Some typical end uses for this product would be electrical products, bellows, springs, washers, corrosion resistant equipment.
Phosphorus Bronze Bush (IS:28-1985):
Cu | Sn | Pb | Zn | Fe | Ni | P | Si | Imp | |
PB-1 | Rem. | 6-8 | 0.25 | 0.5 | 0.3 | 0.7 | 0.3-0.5 | 0.02 | 1.2 |
PB-2 | Rem. | 10 min | 0.25 | 0.05 | 0.1 | 0.1 | 0.5 min | 0.02 | 0.6 |
PB-3 | Rem. | 6.5-8.5 | 2-5 | 2 | - | 1 | 0.3 min | - | 0.8 |
PB-4 | Rem. | 9-11 | 0.25 | 0.05 | - | 0.25 | 0.15 | - | 0.8 |
PB-5 | Rem. | 11-13.1 | 0.5 | 0.3 | 0.15 | 0.5 | 0.15 min | 0.02 |
0.2 |